Novodur Ultra 4255 combines high impact strength at room as well as at low temperature, 100 % ductility at -30 °C, high heat resistance and a best in class flowability. Low temperature ductility, High impact strength, High heat resistance, Good flowability, Low emission. Applications: Door panel, Lower seat trim, Center and overhead console, Glove box door and frameInformation provided by Styrolution. |