MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Phillips 66 Super Lube M EP Grease NLGI No. 2
Categories: Fluid; Lubricant; Lithium Gellant; Organic Soap Gellant

Material Notes: Description: Conoco Super Lube M EP Grease is a premium-quality, multipurpose, high-temperature, extreme-pressure (EP) lithium complex grease developed to satisfy the severe requirements of off-road equipment manufactured by Caterpillar, Komatsu-Dresser, J.I. Case, John Deere and others. These include bulldozers, scrapers, off-highway trucks, wheel loaders, pipelayers, skidders, motor graders and soil compactors where the chassis components and wheel bearings are subjected to heavy loading. Super Lube M EP Grease is also recommended for use in automotive and commercial applications such as chassis, wheel bearings, water pump bearings, universal joints, constant velocity joints, brake self-adjusting screws, tractor-trailer fifth wheels and clutch release bearings. Super Lube M EP Grease also can be used in heavily loaded antifriction and plain bearings used in gear boxes and electric motors. These are commonly found in steel, chemical and aluminum manufacturing plants, where the manufacturer specifies a lithium or lithium complex EP corrosion-resistant grease with moly.

Information provided by ConocoPhillips.

Phillips 66 Lubricants was spun-off from ConocoPhillips in 2012.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Kinematic Viscosity at 40°C (104°F) 200 cStBase Oil
Kinematic Viscosity at 100°C (212°F) 14.5 cStBase Oil
 
Mechanical PropertiesOriginal ValueComments
Four Ball Extreme Pressure, Load Wear Index 60
Four Ball Extreme Pressure, Weld Load 500 kg
Four Ball Wear 0.460 mm
Penetration P(60), 1/10 mm 280
Timken Test 60.0 lb
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 375 °F
Minimum Service Temperature, Air 10.0 °F
Dropping Point >= 500 °F
 
Descriptive Properties
ASTM Rust Fresh and SaltwaterPass
ColorGray-Black
Molybdenum Disulfide3 wt.%
Oil Separation0.21 wt.% Loss
Oxidation Stability7 psi drop/100 hrs
Roll Stability4.2% change in consistency
Soap Type (Thickener)Lithium Complex
Water Washout1.6 %175°F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WCON218 / 75255

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.