MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Daikin DAI-EL® G-801 Fluoroelastomer Copolymer, 66% Fluorine Content
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer

Material Notes: Good low-temperature and elasticity characteristics

Information provided by Daikin.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.80 g/cc
Mooney Viscosity 40
@Temperature 121 °C
ML1+10
 52
@Temperature 100 °C
Compound, ML1+10
 66
@Temperature 100 °C
ML1+10
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 67peak
 61
@Time 3.00 sec
 65
@Treatment Temp. 250 °C,
Time 252000 sec
Air aging test
 66
@Treatment Temp. 230 °C,
Time 252000 sec
Air aging test
Tensile Strength at Break 21.5 MPa
 11.8 MPa
@Treatment Temp. 250 °C,
Time 252000 sec
Air aging test
 16.6 MPa
@Treatment Temp. 230 °C,
Time 252000 sec
Air aging test
Elongation at Break 450 %
 491 %
@Treatment Temp. 230 °C,
Time 252000 sec
Air aging test
 590 %
@Treatment Temp. 250 °C,
Time 252000 sec
Air aging test
100% Modulus 2.00 MPa
@Strain 100 %
Tear Strength 43.0 kN/mangle type
Compression Set 16 %
@Temperature 100 °C,
Time 252000 sec
P-24 O-ring
 16 %
@Temperature 150 °C,
Time 252000 sec
P-24 O-ring
 20 %
@Temperature 50.0 °C,
Time 252000 sec
P-24 O-ring
 21 %
@Temperature 25.0 °C,
Time 252000 sec
P-24 O-ring
 22 %
@Temperature 175 °C,
Time 252000 sec
P-24 O-ring
 30 %
@Temperature 200 °C,
Time 252000 sec
P-24 O-ring
 
Thermal PropertiesOriginal ValueComments
Minimum Service Temperature, Air -19.0 °CLow Temperature Retraction, TR10
 -17.0 °CGehman Torsion T10
 -11.0 °CGehman Torsion T2
 -11.0 °CLow Temperature Retraction, TR70
Brittleness Temperature -25.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 2.50 min
@Temperature 160 °C
Curelastometer, T90
 3.50 min
@Temperature 160 °C
MDR, T90
 
Component Elements PropertiesOriginal ValueComments
Fluorine, F 66 %
 
Descriptive Properties
Test Formula1.5Peroxide
 100Polymer
 20N990 Carbon Black
 4TAIC

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Daikin DAI-EL® G-755 Fluoroelastomer Copolymer, Bisphenol Curable Grade, 66% Fluorine Content
Daikin DAI-EL® G-755 Fluoroelastomer Copolymer, 66% Fluorine Content
Daikin DAI-EL® G-801 Fluoroelastomer Terpolymer, 66% Fluorine Content
Phillips 66 Bentone NLGI Grade 2
Daikin DAI-EL® G-723 Fluoroelastomer Copolymer, Bisphenol Curable Grade, 66% Fluorine Content

PDAIJ9958 / 210031

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.