MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Lanxess LEWATIT® NM 60 SG Ion Exchange Resin
Categories: Polymer; Thermoset

Material Notes: Lewatit® NM 60 SG is a premium grade, gel type, high capacity, high purity mixed ion exchange resin prepared with a 1:1 chemically equivalent ratio of cation to anion resin. Lewatit NM 60 SG is a mixture of gel type cation exchange resin in the hydrogen (H) form, and a gel type anion exchange resin in the hydroxide (OH) form. The mixed resin is prepared from component resins which have been manufacture with the highest degree of purity and conversion to the H/OH form. Lewatit NM 60 SG is supplied pre-mixed as spherical beads in a heterodispersed particle distribution in the fully swollen bead form. Lewatit NM 60 SG is specially prepared to provide a rapid rinse up to a resistivity of18+ megohm*cm, and to provide a rapid rinse in for Total Organic Carbon (TOC). Lewatit NM 60 SG should provide +18 megohm*cm quality within 80 BV of rinse water, and <3 ppd delta TOC within 50 BV rinse water. Lewatit NM 60 SG is designed to reliably provide UPW quality water for microelectronics, laboratory, one-through cartridges, and high purity service-exchange applications. Lewatit NM 60 SG is designed for non-regenerable application. The component resins can be separated, and regenerated and remixed, however, the treated water quality after user regeneration may not be of the same high purity as the virgin supplied resin.

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.688 g/cc
Density 1.10 g/cc
Bead Size 0.300 - 1.25 mm>90%
Storage Temperature 4.00 - 24.0 °C
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 60.0 °C
 
Descriptive Properties
AppearanceBrown, translucent
pH Operating Range0 - 14

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLANY8813 / 209205

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.