MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Sharadaa Ceramics REFCAST NORMAL Dense Castables
Categories: Ceramic

Material Notes: Manufacturer offers a range of Dense Castables that are conventional castable and extensively used in boiler work, general furnace and burner blocks. Made as per international standards, our range is known for its high strength, low thermal conductivity and requires less maintenance.

Information provided by Sharadaa Ceramics Pvt. Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density >= 2.00 g/ccSample, cast, cured, dried at 110°C
Grain Size <= 5000 µm
 
Mechanical PropertiesOriginal ValueComments
Compressive Strength 250 kg(f)/cm²
@Temperature 1100 °C
Cold Crushing
 350 kg(f)/cm²
@Temperature 110 °C
Cold Crushing
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 1300 °C
 
Processing PropertiesOriginal ValueComments
Moisture Content 12 - 14 %
 
Component Elements PropertiesOriginal ValueComments
Al2O3 >= 45 %
Fe2O3 <= 5.0 %
 
Descriptive Properties
Permanent Linear Change-1.0 - 1.0%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

CSHARA012 / 130175

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.