MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Borealis FR4847 Polyethylene Based Striping Compound
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: FR4847 is a Polyethylene Based Striping Compound for Primary Automotive Wires. FR4847 is designed and manufactured with advanced material and processing technology to provide enhanced stabilization and lower particulate matter. This compound was designed to have high compatibility with our chemically crosslinkable non-halogen flame retardant insulation compounds. Application: FR4847 is intended for use as non-halogen flame retardant polyethylene compound in striping applications for primary automotive wires. It would be used in conjunction with our chemically crosslinkable nonhalogen flame retardant insulation compounds.

Information provided by Borealis AG

Key Words: PE
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.40 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 48ASTM D2240
Tensile Strength at Break 9.00 MPaASTM D412
Elongation at Break 280 %
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+6 ohm-cmASTM D257
Dielectric Constant 3.7
@Frequency 6e+7 Hz
ASTM D150
Dielectric Strength >= 22.0 kV/mm
Dissipation Factor 0.010
@Frequency 6e+7 Hz
ASTM D150
 
Processing PropertiesOriginal ValueComments
Middle Barrel Temperature 121 °C
Melt Temperature 120 - 125 °C
Drying Temperature 55.0 °Cdrying;2-8h
Shelf Life 12.0 Month

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PBOREA449 / 108708

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.