MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Lanxess Aktiplast® T Processing Aid
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Function: Peptizer for natural and isoprene rubber as well as for their blends with other synthetic rubbers; processing promoter for synthetic rubber; activator with delayed action

Use: Aktiplast T has got a lower melting range than Aktiplast PP. It becomes effective in natural and isoprene rubber at a mill temperature of 60 °C. Since Aktiplast T is soluble in rubber, a homogeneous breakdown is achieved without the risk of blooming. Aktiplast T prolongs the scorch time and serves as a dispersing agent for all fillers. Owing to its zinc content, Aktiplast T activates the vulcanization. The addition of stearic acid is not necessary, a reduction of zinc oxide is possible. Aktiplast T reduces the mixing time and improves the flow characteristics of the uncured compound. Aktiplast T has no adverse effect on rubber-to-metal bonding. Aktiplast T improves the storage stability, which is of particular advantage in direct vulcanization.

Application: Molded and extruded goods of all types, expanded rubber articles, solid rubber. Peptizing effect in NR and IR above 60 °C. Retards scorch and accelerates vulcanization.

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.05 g/cc
Ash 12 - 14 %
 
Thermal PropertiesOriginal ValueComments
Melting Point 78.0 - 96.0 °C
 
Processing PropertiesOriginal ValueComments
Shelf Life 36.5 Month
 
Descriptive Properties
Appearancebrown Pellets

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lanxess Aktiplast® Processing Aid
Lanxess Aktiplast® 2635 Processing Aid
Lanxess Aflux® 42 Processing Aid
Lanxess Aflux® 42 M Processing Aid
Lanxess Aflux® 42 M pellets Processing Aid

PLANY8255 / 208648

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.