MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ITW Devcon® Dev-Thane™ 5 Polyurethane Adhesive
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: A two-part, fast setting. Primer less high performance urethane adhesive for bonding many different substrates such as steel, aluminum, ABS, urethane, and composites. Uses: Bonds steel, aluminum, stainless steel, galvanized steel, concrete, wood, glass, ABS, and urethanes with no primers.

Information provided by ITW Performance Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.0510 lb/in³
 11.75 lb/galuncured
Solids Content 100 %
Viscosity 45000 cPCuring Agent
 45000 cPMixed
 45000 cPResin
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 63
Tensile Strength 2100 psi
Elongation at Break 200 %
Adhesive Bond Strength 630 psi[ABS]. Cured 7 days @ 75°F. Substrate failure. Lap Shear; ASTM D1002
 895 psi[SMC]. Cured 7 days @ 75°F. Lap Shear; ASTM D1002
 1200 psi[Concrete]. Cured 7 days @ 75°F. Lap Shear; ASTM D1002
 1270 psi[AL]. Cured 7 days @ 75°F. Lap Shear; ASTM D1002
 1575 psi[Galvanized metal]. Cured 7 days @ 75°F. Lap Shear; ASTM D1002
 1840 psi[SS]. Cured 7 days @ 75°F. Lap Shear; ASTM D1002
 2750 psi[GBS]. Cured 7 days @ 75°F. Lap Shear; ASTM D1002
Tear Strength 400 pliASTM D624
Peel Strength 65.0 - 75.0 pliASTMf D1876
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 13.8 kV/mmASTM D149
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 200 °F
Minimum Service Temperature, Air -40.0 °F
Shrinkage 0.14 %Linear During cure; ASTM D2566
 
Processing PropertiesOriginal ValueComments
Cure Time 4.00 hourFunctional
 24.0 hourFull
 168 hour
@Temperature 24.0 °C
As Tested
Pot Life 5.00 min
@Temperature 23.9 °C
 
Descriptive Properties
Chemical/Solvent ResistanceCutting Oil: excellent30 day immersion at 75°F. Sample cured 7 days at RT
 Gasoline (unleaded): fair30 day immersion at 75°F. Sample cured 7 days at RT
 Hydrochloric Acid 10%: excellent30 day immersion at 75°F. Sample cured 7 days at RT
 Isopropanol: fair30 day immersion at 75°F. Sample cured 7 days at RT
 Methyl Ethyl Ketone: poor30 day immersion at 75°F. Sample cured 7 days at RT
 Motor Oil: excellent30 day immersion at 75°F. Sample cured 7 days at RT
 Sodium Chloride Brine: excellent30 day immersion at 75°F. Sample cured 7 days at RT
 Sodium Hydroxide 10%: excellent30 day immersion at 75°F. Sample cured 7 days at RT
 Toluene: poor30 day immersion at 75°F. Sample cured 7 days at RT
ColorGrayUncured
Coverage300 in²/50mLUncured, @ 0.01"
Gap Filling (in)good
Mix Ratio by volume1:1
Mix Ratio by weight1:1
Specific Volume (in.³/lb)19.6

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PITWD9215 / 239724

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.