MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Go Yen Chemical GY-DG-84 Highly Effective Degradable & Decompositional Additive for Plastic
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Intro: GO YEN CHEMICAL INDUSTRIAL CO. LTD. (GYC) has been focus on the highest end & environmental innovation and R&D for a long time. GY-DG-84 offers a complete range of solutions for the defects of traditional degradable materials, such as high price of PLA/less of applications/cannot combine with the general plastic, etc. The concept of degradable plastic refers to: It can be decomposed into small molecules polymer by microorganisms from sun or soil in the short time after getting the expired time of plastic product. The delayed period of degradable plastic which means it is from the beginning of processed into plastic product to a small transverse cracks in time by the external environmental conditions. Different degradable with the different delayed period?the requirement length for delayed period of various plastic is also different. As the example, the delayed period of plastic film is not less than the growing season of crops. GYC Nano decomposable material not only has high efficiency degradation ability but also provides the following advantages:
  • Can use compound and add in the variety of plastic: PP.LDPE.HDPE.LLDPE.…etc.
  • Less efficient usage rate and achieve large number of applications of degradable plastic for human
  • The degradation delayed period fixed and appropriated length, it can control the start time of degradable plastic
  • High decomposition speed, it can be degraded by environment, soil, sunlight, humidity, UV light and the oxygenation in the air after used
  • PLA material which made by natural corn or starch is an expensive, low heat resistant product. Moreover, this item can’t be used widely. Comparing with PLA, GY-DG-84 has well price performance ratio.
  • PLA materials need a special environment at high temperature 50 ° C, humidity 50% ~ 60%, it also takes about 40 days to decompose naturally, difficult to decompose in open-air environment
  • The recycle of PLA should be separated and classified exactly, it will increase the cost and time of recycle
  • Can be combined with traditional petrochemical products such as :PP.PE. LDPE.HDPE.LLDPE…etc
Applications:
  • Polyolefin film products
  • Plastic: PP, PE, LDPE, HDPE, LLDPE, EVA
  • Engineering plastic: PC.PET.PBT.ABS
  • Agricultural mulch film
  • Agricultural film
  • Bags
  • Shopping bags
  • Building packaging film
  • Garbage bags
  • Other senior degradable products application

Information provided by Go Yen Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Particle Mesh Size 200 Mesh0.99
 
Thermal PropertiesOriginal ValueComments
Melting Point >= 85.0 °C
 
Descriptive Properties
AppearancePowder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PGOYEN341 / 266649

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.