MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Avient PolyOne® CPE UV Res. Nat 1240 Chlorinated Polyethylene (CPE)  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes:

An excellent choice for low-voltage power-and-cable control cables, this filled, flexible thermoplastic CPE jacketing compound offers wire and cable manufacturers the advantages of thermoplastic extrusion processing without the need to invest in continuous vulcanization (CV) equipment. CPE 30-11 REV 2 is excellent for larger-diameter cable. This compound passes testing for heat/shock resistance, which requires cable to withstand being bent and twisted without cracking or showing stress. Good moisture, oil, and electrical properties. Applications include power-and-control cable for fossil-fuel and co-generation plants.

Applications:

  • Power and Control Cable Jacket

Market:

  • Wire & Cable
PolyOne First Choice

Disclaimer: Note: Typical processing temperatures range between 320°-390°F depending upon screw design. Contact Technical Service for recommendation for specific equipment.
Note: Pre-drying is recommended for 8-24 hours at 175°-185°F.
NOTE: Typical Properties of Molded Slab (0.075"); Not to be Construed as Specifications.

Information provided by PolyOne Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.32 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 4810 Sec; ASTM D2240
Tensile Strength at Break 2275 psi168 hrs (7 days), 250°F(121°C), Type 4 - Flexibles, Break, 2 in/min; ASTM D3045
 2427 psiType 4 - Flexibles, Break, 20 in/min; ASTM D638
Elongation at Break 520 %Type 4 - Flexibles, 20 in/min; ASTM D638
Tensile Modulus 1312 psiType 4 - Flexibles, 20 in/min; ASTM D638
 
Thermal PropertiesOriginal ValueComments
Oxygen Index 33 %0.075 in; ASTM D2863
 
Descriptive Properties
AppearancePellets/CubesASTM D2090
Heat Shock, 1 hr @ 150° CPassIEC 60811-3-1
Immersion- Elo. variation from Orig.87.5%IRM 902 OIL, 24 hrs @ 70°C, IEC 60811-2-1
Immersion- TS variation from Orig.59.7%IRM 902 OIL, 24 hrs @ 70°C, IEC 60811-2-1

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PH1PO3458 / 45087

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.