MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
CHT EM 1039 Emulsion
Categories: Other Engineering Material

Material Notes: Introduction: Emulsion EM 1039 is a water dilutable 35% silicone fluid emulsion, employed as a releasing agent for rubber and generally plastic materials. In art graphic industry it is mainly used as antistatic and slip agent, it confers resistance to scratching during paper folding processes and protection to mechanical components.

Key features

  • General purpose release agent
  • Minimum build-up on mould
  • Moulded parts not discoloured
  • Good dilution stability
  • Good lubricant and antistatic properties
  • Chemically inert
Applications: Emulsion EM 1039 has been formulated specially as a release agent and lubricant in a wide range of applications and processes such as:
  • mould release agent
  • release agent for bandaging of rubber tubes in vulcanisation process
  • textile lubricant for yarn and thread as well as hosiery manufacture
  • lubricant and antistatic in rotogravure off-set printing
  • release agent for plastic tubes used to form bags and sacks
  • gloss, slip and wettability in detergent and cleaner formulations

Information provided by CHT Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.980 g/ccBS 5350 Part B1
Solids Content 37 - 39 %
pH 6.5 - 8.5
Brookfield Viscosity 350 cP
Storage Temperature 5.00 - 30.0 °C
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month
 
Descriptive Properties
% actives34-36%
AppearanceLiquid
IonicityNon-ionic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCHTSIL336 / 314819

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.