MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LyondellBasell Adflex V 109F Thermoplastic Polyolefin
Categories: Polymer; Film; Thermoplastic; Polyolefin

Material Notes: Adflex V 109 F is a reactor TPO (thermoplastic polyolefin) manufactured using LyondellBasell's proprietary Catalloy process technology. It is primarily used for molding, impact modification, extrusion coating and film applications. This resin can be used on conventional injection molding or extrusion equipment. Adflex V 109 F features a very high softness and low modulus, with a relatively high melt flow. The grade is available in natural pellet form. Applications: Automotive Flooring, Film Wrap, House wares, Industrial, Specialty Film, Sports, Leisure & Toys, TPO Residential Flooring.

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.880 g/ccMethod A; ISO 1183-1
Melt Flow 12 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133-1
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 30
@Time 15.0 sec
ISO 868
Tensile Strength at Break 8.00 MPaISO 527-1,-2
Tensile Strength, Yield 5.00 MPaISO 527-1,-2
Elongation at Break 800 %ISO 527-1,-2
Elongation at Yield 40 %ISO 527-1,-2
Flexural Modulus 80.0 MPaISO 178
Charpy Impact, Notched 1.40 kJ/m²
@Temperature -40.0 °C
failure mode: complete break; ISO 179
 5.00 kJ/m²
@Temperature -20.0 °C
failure mode-partial break; ISO 179
 35.0 kJ/m²
@Temperature 23.0 °C
failure mode-partial break; ISO 179
Tear Strength 65.0 kN/mASTM D624
 
Thermal PropertiesOriginal ValueComments
Melting Point 142 °CDSC; ISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 35.0 °Cunannealed; ISO 75B-1,-2
Vicat Softening Point 55.0 °CA50; ISO 306
 
Optical PropertiesOriginal ValueComments
Haze 49 %
@Thickness 1.14 mm
ASTM D1003
Gloss 62 %
@Thickness 1.14 mm
@60°; ASTM D2457
 
Descriptive Properties
Processing MethodCast Film; Compounding; Injection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEQT7007 / 218646

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.