MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Röchling DuroProtect® 1000 Anti-Ballisitc Sheet
Categories: Polymer; Thermoplastic

Material Notes:
  • Bullet Resistant Material
  • UL® Recognized
  • UL-752 Levels 1-5, and 8 Outdoor Rating
  • UL-94 V0 Flame Rating
  • Lightweight
  • Military and Commercial Applications
DuroProtect® is a thin and lightweight composite panel that has been recognized by Underwriters Laboratories to meet their UL-752 specifications for bullet resisting plastics. (Levels 1-5 and 8). DuroProtect® has been rated to stop threats form a multitude of firearms tested in various conditions and shot patterns at short range. DuroProtect® is designed to provide protection from bullets and other projectiles. DuroProtect® can be used in a variety of applications where personal and property protection is required or desired. Threat level 4,5 and 8 panels can be achieved by bonding a combination of the other threat levels together or can be molded to thickness. Both were tested and meet the requirements of UL-752.

Applications:

  • Government Buildings
  • Drive-up Bank Tellers
  • ATM’s
  • Guard Houses
  • Safe Rooms
  • Vehicle Armor
  • Schools/Classrooms
  • Window Shutters/Storm Shelters
  • Convenience Stores
  • Gas Stations
  • Courtrooms
  • Toll Booths
  • Others

Information provided by Röchling.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.00 g/ccASTM D792
Water Absorption <= 1.4 %ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Hardness, Barcol 50ATM D2583
Tensile Strength 276 MPaCW; ASTM D638
 310 MPaLW; ASTM D638
Tensile Modulus 3.75e+6 psiASTM D638
Flexural Strength 16800 psiLW; ASTM D790
Flexural Modulus 2.70e+6 psiLW; ASTM D790
Compressive Strength 70000 psiASTM D695
Izod Impact, Notched 52.0 ft-lb/inASTM D256
 
Thermal PropertiesOriginal ValueComments
CTE, linear 20.0 µm/m-°CASTM D696
Thermal Conductivity 0.288 W/m-KASTM C177
Flammability, UL94 V-0
 
Descriptive Properties
ColorOff White

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Covestro Makrolon® 2800 Polycarbonate
Covestro Makrolon® 2807 Polycarbonate, Injection Grade
Covestro Bayblend® T85 XF Polycarbonate + ABS
Chi Mei Polylac® PA-765A ABS - Flame Retardant
Covestro Makrolon® 8345 Polycarbonate

PROCH9372 / 233074

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.