MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Inov Chem Donfoam 813 CP/IP Base blend polyols
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Donfoam813 blend polyols use CP or CP/IP as blowing agent ,used in the production of high flame retardant PIR block foam, with performances of uniform foam cell , low thermal conductivity, good thermal insulation and flame retardant, low temperature no shrinking crack etc. Widely used in the process of all kinds of insulation work such as: building external wall, cold storage, tanks, large pipes etc.

Information provided by Shandong INOV Polyurethane Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.19 - 1.21 g/cc
Density 0.0280 - 0.0350 g/ccFree density, Manual mixing
 >= 0.0400 g/ccMolding Core Density; ASTM D1622
 >= 0.0500 g/ccOverall Molding Density; ASTM D1622
Water Absorption <= 3.0 %ASTM D2842
Viscosity 400 - 600 cPDynamic
Storage Temperature 10.0 - 25.0 °C
 
Mechanical PropertiesOriginal ValueComments
Compressive Strength >= 0.150 MPaASTM D1621
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity <= 0.0240 W/m-K
@Temperature 15.0 °C
ASTM C518
 
Processing PropertiesOriginal ValueComments
Processing Temperature 20.0 - 25.0 °CRaw material temperature, Manual mixing
Mold Temperature 15.0 - 45.0 °CAmbient Temperature, Manual mixing
Cure Time 240 - 360 secTack free time, Manual mixing
Gel Time 2.30 - 3.30 minManual Mixing
Shelf Life 6.00 Month
 
Descriptive Properties
AppearanceLight yellow to brown transparent liquid
Closed-cell rate=90%ASTM D2856
Cream time35-60 sec
Dimensional stability=1.0%24h, -20?; GB/T8811
 =1.5%RH90 70?; GB/T8811
Recommended Ratio100Blend Polyols
 11-13CP or CP/IP
 140-150Isocyanate

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PINOVCHM030 / 312559

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.