MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Teknor Apex Duramid TH7G12.2S*9207 Nylon 66 + 6I/6T, Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Unreinforced

Material Notes: Notes: R106/N/50GFS is a 50% glass fiber reinforced nylon 6 that offers excellent mechanical performance coupled with good surface finish.

Availability: Europe; North America

Fillers/Reinforcement: Glass Fiber, 50% Filler by Weight

Features: Good Surface Finish

Processing Method: Injection Molding

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.72 g/ccISO 1183
Water Absorption 0.30 %
@Time 86400 sec
ISO 62
Water Absorption at Saturation 2.0 %ISO 62
Linear Mold Shrinkage, Flow 0.0020 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.0040 in/inISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 37700 psiISO 527-2
Elongation at Break 2.5 %ISO 527-2
Tensile Modulus 3.63e+6 psiISO 527-2
Flexural Strength 20800 psiISO 178
Flexural Modulus 2.68e+6 psiISO 178
Izod Impact, Notched (ISO) 9.50 ft-lb/in²ISO 180
Charpy Impact Unnotched 31.0 ft-lb/in²
@Temperature -30.0 °C
ISO 179
 31.0 ft-lb/in²
@Temperature 22.8 °C
ISO 179
Charpy Impact, Notched 9.50 ft-lb/in²
@Temperature -30.0 °C
ISO 179
 9.50 ft-lb/in²
@Temperature 22.8 °C
ISO 179
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 990 V/mil
@Thickness 2.00 mm
IEC 60243-1
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 491 °FUnannealed; ISO 72-2/B
Deflection Temperature at 1.8 MPa (264 psi) 473 °FUnannealed; ISO 72-2/A
Vicat Softening Point 446 °FISO 306/B
 482 °FISO 306/A
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 554 °F
Melt Temperature 509 °FISO 11357-3
Mold Temperature 176 - 248 °F
Drying Temperature 176 °F
Dry Time 2.00 - 4.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTEKNQ0625 / 237116

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.