MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Elmet Technologies Pure Molybdenum Wire
Categories: Metal; Nonferrous Metal; Molybdenum Alloy; Refractory Metal; Pure Element

Material Notes: The chemical composition complies with ASTM requirements for powder lot analysis. Actual finished part chemical analysis and mechanical properties are not routinely evaluated per ASTM requirements. ASTM specifications and test methods are used as guidelines to control and monitor production processes to assure product quality. Applicable ASTM Material Standards: B387-90 (re-approved 1995) for rod/wire. This product meets the requirements of low copper and mercury-free materials.

Information provided by Elmet Technologies.

Vendors: Elmet Technologies is a 100% US owned and operated, fully integrated manufacturer of Molybdenum, Tungsten and related alloys such as TZM, WHA & MoLa. At our 220,000 sqr/ft plant in Lewiston, Maine, Elmet manufactures W & Mo pure powders plus rod, wire, plate, sheet & foil in additional to offering fabrication and machining services. ITAR, ISO and AS9100 registered. www.elmettechnologies.com

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 10.22 g/cc
a Lattice Constant 3.1399 Å
Vapor Pressure 7.58e-023 torr
@Temperature 787 °C
 1.00e-17 torr
@Temperature 927 °C
 2.58e-12 torr
@Temperature 1227 °C
 7.88e-10 torr
@Temperature 1527 °C
 0.000154 torr
@Temperature 2127 °C
 0.0180 torr
@Temperature 2727 °C
 1.58 torr
@Temperature 3227 °C
 
Chemical PropertiesOriginal ValueComments
Atomic Mass 95.94
Atomic Number 42
Atomic Volume 9.41[cc/gm atom]
 
Mechanical PropertiesOriginal ValueComments
Modulus of Elasticity 46000 ksi
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000552 ohm-cm
@Temperature 27.0 °C
 0.00000740 ohm-cm
@Temperature 100 °C
 0.00001315 ohm-cm
@Temperature 327 °C
 0.0000171 ohm-cm
@Temperature 500 °C
 0.0000222 ohm-cm
@Temperature 700 °C
 0.00002951 ohm-cm
@Temperature 927 °C
 0.00003814 ohm-cm
@Temperature 1227 °C
 0.00004702 ohm-cm
@Temperature 1527 °C
 0.00005306 ohm-cm
@Temperature 1727 °C
 0.00005918 ohm-cm
@Temperature 1927 °C
 0.00006537 ohm-cm
@Temperature 2127 °C
 0.00007161 ohm-cm
@Temperature 2327 °C
 0.0000779 ohm-cm
@Temperature 2527 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 5.20 µm/m-°C
@Temperature 20.0 °C
 5.80 µm/m-°C
@Temperature 2000 °C
 6.50 µm/m-°C
@Temperature 2500 °C
Specific Heat Capacity 0.270 J/g-°C
Thermal Conductivity 0.200 cal cm/sec-cm²-°C
@Temperature 1500 °C
 0.250 cal cm/sec-cm²-°C
@Temperature 1000 °C
 0.290 cal cm/sec-cm²-°C
@Temperature 500 °C
 0.330 cal cm/sec-cm²-°C
@Temperature 100 °C
 0.340 cal cm/sec-cm²-°C
@Temperature 20.0 °C
Melting Point 2610 °C
Boiling Point 4612 °C
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al <= 0.0025 %
Cadmium, Cd <= 0.0015 %
Calcium, Ca <= 0.0020 %
Carbon, C <= 0.0050 %
Chromium, Cr <= 0.0020 %
Copper, Cu <= 0.0010 %
Iron, Fe <= 0.0050 %
Lead, Pb <= 0.0010 %
Magnesium, Mg <= 0.0010 %
Molybdenum, Mo >= 99.95 %
Nickel, Ni <= 0.0050 %
Nitrogen, N <= 0.0020 %
Other, each <= 0.0020 %
Oxygen, O <= 0.0050 %
Potassium, K <= 0.0030 %
Silicon, Si <= 0.0025 %
Sodium, Na <= 0.0020 %
Tin, Sn <= 0.0020 %
Tungsten, W <= 0.030 %
 
Descriptive Properties
Electron Work Function4.2 eV
Lattice StructureBody Centered Cubic
RoHS Compliance2002/95/EC

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

NELMET924 / 242045

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.