MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
JIS SKC11 Low-Alloy Tool Steel
Categories: Metal; Ferrous Metal; Tool Steel

Key Words: JIS G4410(84) SKC11, STC 11, SKC-11; Comparable to SKT3, AISI L2 Tool Steel, UNS T61202
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.86 g/cc(AISI L2)
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 285 - 375Rod or Bit Fully Killed
 
Thermal PropertiesOriginal ValueComments
CTE, linear 11.3 µm/m-°C(AISI L2)
 
Processing PropertiesOriginal ValueComments
Processing Temperature 175 - 315 °CTempering Temperature (AISI L2)
 845 - 925 °CHardening Temperature (AISI L2)
Annealing Temperature 760 - 790 °C(AISI L2)
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.85 - 1.1 %
Chromium, Cr 0.80 - 1.5 %
Copper, Cu <= 0.25 %
Iron, Fe 95.4 - 98.2 %As Balance
Manganese, Mn <= 0.50 %
Molybdenum, Mo <= 0.40 %
Nickel, Ni <= 0.20 %
Phosphorus, P <= 0.030 %
Silicon, Si 0.15 - 0.35 %
Sulfur, S <= 0.030 %
Vanadium, V <= 0.25 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AISI 1064 Steel, hot rolled, 19-32 mm (0.75-1.25 in) round
AISI Type L2 Low-Alloy Tool Steel (UNS T61202)
Overview of materials for Cold Work Steel
Overview of materials for Hot Work Steel
Bohler-Uddeholm UDDEHOLM MIRRAX ESR Plastic Mold Steel

MSTZJSKC11 / 231076

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.