MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
SABIC LNP™ ELCRES™ ML4412 Polycarbonate (PC)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: LNP ELCRES ML4412 is based on Polycarbonate (PC) siloxane copolymer resin containing 20% glass fiber, medium flow, impact modified injection moldable grade. This grade is available in opaque colors only and is an excellent candidate for a broad range of applications that require a combination of stiffness and ductility.

Features: Impact Modified,High Stiffness

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.33 g/ccASTM D792
Density 1.33 g/ccISO 1183
Moisture Absorption 0.0200 %Injection Molding
 0.0300 %23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.10 %ISO 62-1
Viscosity 10 cP
@Load 1.20 kg,
Temperature 300 °C
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0020 - 0.0030 cm/cm
@Thickness 3.20 mm
SABIC method
Linear Mold Shrinkage, Transverse 0.0040 - 0.0050 cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow 11 g/10 min
@Load 1.20 kg,
Temperature 300 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 100 MPa50 mm/min; ASTM D638
 110 MPa50 mm/min; ISO 527
Elongation at Break 3.0 %50 mm/min; ASTM D638
 3.0 %50 mm/min; ISO 527
Tensile Modulus 6300 MPa50 mm/min; ASTM D638
 6500 MPa1 mm/min; ISO 527
Flexural Strength 160 MPayld, 1.3 mm/min, 50 mm span; ASTM D790
 165 MPayield, 2 mm/min; ISO 178
Flexural Modulus 5700 MPa2 mm/min; ISO 178
 5800 MPa1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched 140 JASTM D256
Izod Impact, Unnotched 700 J/mASTM D4812
Izod Impact, Notched (ISO) 17.0 kJ/m²80*10*3; ISO 180/1A
 12.0 kJ/m²
@Temperature -30.0 °C
80*10*3; ISO 180/1A
Charpy Impact, Notched 17.0 kJ/m²Edgew 80*10*3 sp=62mm; ISO 179/1eA
 12.0 kJ/m²
@Temperature -30.0 °C
Edgew 80*10*3 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 25.0 JASTM D3763
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 3.11
@Frequency 1.10e+9 Hz
ASTM ES 7-83
 3.13
@Frequency 1.90e+9 Hz
SABIC method
 3.14
@Frequency 5.00e+9 Hz
SABIC method
 3.16
@Frequency 1e+10 Hz
SABIC method
Dissipation Factor 0.0051
@Frequency 5.00e+9 Hz
SABIC method
 0.0060
@Frequency 1.90e+9 Hz
SABIC method
 0.0063
@Frequency 1e+10 Hz
SABIC method
 0.0064
@Frequency 1.10e+9 Hz
ASTM ES 7-83
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 26.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
CTE, linear, Transverse to Flow 68.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
Deflection Temperature at 0.46 MPa (66 psi) 137 °CEdgew 120*10*4 sp=100mm; ISO 75/Be
 135 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 133 °CEdgew 120*10*4 sp=100mm; ISO 75/Ae
 132 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Vicat Softening Point 142 °CRate B/120; ISO 306
UL RTI, Electrical 80.0 °CUL 746B
UL RTI, Mechanical with Impact 80.0 °CUL 746B
UL RTI, Mechanical without Impact 80.0 °CUL 746B
Flammability, UL94 HB
@Thickness >=0.400 mm
UL 94
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 285 - 305 °C
Zone 2 270 - 290 °C
Zone 3 280 - 300 °C
Melt Temperature 285 - 310 °CInjection Molding
Mold Temperature 80.0 - 110 °C
Drying Temperature 110 °CInjection Molding
Dry Time 3.00 - 6.00 hourInjection Molding
Back Pressure 0.100 - 0.300 MPa
Screw Speed 50 - 90 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH80597 / 288544

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.