WF-9942 Wave Soldering Flux is a no-clean flux specifically developed for wave soldering, mixed-technology and through-hole electronic assemblies. This formulations provides greater heat stability required for the increases temperatures used in Pb-free wave soldering processes. WF-9942 is formulated to provide a wide process window with excellent solderability, superior hole-fill and reduced solder balling on all surface finishes. this product can be used with Sn/Cu, Sn/Ag/Cu and Sn/Pb alloys.Features: - Use with Pb-free and Sn/Pb alloys
- Excellent solderability on all board finishes
- Superior hole-fill
- Reduces solder balling
Physical Properties - Color: Clear
- J-STD-004 Flux Type: ORL0
Information Provided by Indium Corporation |