Description: VTA®266 is 65 to 120°C (150 to 250°F) curing, gray surface improvement film compatible with Cyctec’s VTM®260 series Out-of-Autoclave (OoA) prepregs. VTF266 can be supplied on a number of carriers/scrims. VTF266 molds to a tough, sandable, paint-ready surface directly from the mold. Features & Benefits: - 30 days out life at 21°C (70°F)
- 12 months storage at -18°C (0°F)
- Compatible with the VTM260 series pregregs fro OoA processing
- Can also be autoclave cured
- 65°C (150°F) minimum initial cure
- Good tack and drape
- Molds to a tough, gray, sandable, paint-ready surface
Information provided by Cytec, subsequently acquired by Solvay. |