MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
NatureWorks® Ingeo™ 6350D Fiber Grade PLA
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polylactic Acid (PLA) Biopolymer

Material Notes: NatureWorks® PLA polymer 6350D is an amorphous thermoplastic spunbond-grade resin derived primarily from annually renewable resources. Available in pellet form, 6350D is designed for extrusion into spunbond nonwovens using conventional bi-component PET spunbond equipment, where filament velocities > 4000 m/min can be achieved. NatureWorks® PLA 6350D can be used as a low melt binder polymer in a sheath-core configuration. Potential applications for PLA polymer 6350D include bicomponent spunbond non-wovens

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.24 g/ccASTM D792
Melt Density 1.08 g/cc
@Temperature 230 °C
ASTM D1238
Viscosity Measurement 2.5Relative Viscosity; CD Internal Viscotek Method
Melt Flow 65 g/10 min
@Load 2.16 kg,
Temperature 210 °C
ASTM D1238
 
Thermal PropertiesOriginal ValueComments
Melting Point 145 - 160 °CASTM D3418
Glass Transition Temp, Tg 55.0 - 60.0 °CASTM D3417
 
Processing PropertiesOriginal ValueComments
Dew Point -35.0 °C
Drying Air Flow Rate >= 0.500 ft³/min (CFM)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
NatureWorks® Ingeo™ 6060D Fiber Grade PLA
Total Corbion Luminy LX130U PLA, Biobased Polymer
NatureWorks® Ingeo™ 6201D Fiber Grade PLA
NatureWorks® Ingeo™ 5051X Fiber Grade PLA
NatureWorks® Ingeo™ 4060D Sealant Grade PLA

PNATU97 / 103495

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.