MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Borealis Visico™ LE4481/LE4437 Moisture-Crosslinking Polyethylene Compound for Flexible Low Voltage Insulation  (discontinued **)
Categories: Polymer; Thermoplastic; Ethylene Butyl Acrylate; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Wire/Cable Grade

Material Notes: Visico LE4481/LE4437 is a natural, low-density ethylene vinyl silane/ ethylene butyl acrylate terapolymer that is designed for flexible low voltage wire insulation and jacketing. The combination of a Visico base material, LE4481, and a tine catalyst masterbatch, LE4437, provides a patented scorch retardant additive (SRA) that increases the processing window for a moisture crosslinking compound and minimizes the tendency for premature crosslinking in the extruder, head or die. LE4437 should be added to LE4481 directly in the extruder hopper by dry blending at a ratio of 5 parts LE4437 to 95 parts LE4481. LE4437 also provides, in addition to catalyst, a stabilization package containing suitable antioxidant, a metal passivator and a metal deactivator. Properly mixed, during the extrusion process, LE4481/LE4437 exhibits excellent thermal stability to oxidation.

LE4481/LE4437 is recommended for use as insulation for low voltage control cables and power cables up to 6 kV in rating that require excellent ambient and low temperature flexibility.

Information provided by the Manufacturer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.928 g/ccLE 4481; ASTM D792
 0.933 g/ccLE 4437; ASTM D792
Melt Flow 4.5 g/10 minLE 4481; ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield >= 1440 psiHeat Aging (7 days at 121°C); ASTM D412
 1600 psiASTM D412
Elongation at Break <= 50 %Hot Creep Test (150°C, .2 MPa); ICEA T-28-562
 225 %Heat Aging (7 days at 121°C); ASTM D412
 250 %ASTM D412
Tensile Set <= 5.0 %Hot Creep Test (150°C,.2 MPa); ICE T-28-562
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 1.00e+16 ohm-cmASTM D257
Dielectric Constant <= 2.7
@Frequency 60 Hz
ASTM D150
Dielectric Strength >= 550 V/milASTM D149
Dissipation Factor 0.0010
@Frequency 60 Hz
ASTM D150
 
Processing PropertiesOriginal ValueComments
Middle Barrel Temperature >= 140 °C
Front Barrel Temperature >= 120 °C
Die Temperature >= 285 °F
Head Temperature >= 140 °C

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LyondellBasell Petrothene® GA808093 Linear Low Density Polyethylene
Borealis Visico™ LE4421/LE4437 Scorch Retardant, Moisture-Crosslinking Polyethylene Compound for Low Voltage Installation
RTP Company RTP 101 FR Polypropylene (PP) Glass Fiber - Flame Retardant - UL94 V-0
Mitsubishi Xantar® 19 UR Polycarbonate
Covestro Apec® 1745 Polycarbonate

PBOREA202 / 27509

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.