MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SABIC LNP™ STAT-LOY™ Compound PF303 Polyamide 6 (Nylon 6) (Americas)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6)

Material Notes: LNP STAT-LOY PF303 compound is based on Nylon 6 resin containing 15% glass fiber. Added features of this grade include: Permanently Anti-Static.

Features: Antistatic

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.25 g/ccASTM D792
Density 1.24 g/ccISO 1183
 1.25 g/ccASTM D792
Moisture Absorption 0.150 - 0.250 %Injection Molding
 6.60 %23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm24hrs; ASTM D955
Linear Mold Shrinkage, Transverse 0.0090 - 0.020 cm/cm24hrs; ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 68.0 MPa5 mm/min; ISO 527
 74.0 MPa5 mm/min; ASTM D638
Tensile Strength, Yield 72.0 MPa5 mm/min; ISO 527
 82.0 MPa5 mm/min; ASTM D638
Elongation at Break 2.3 %5 mm/min; ASTM D638
 2.8 %5 mm/min; ISO 527
Elongation at Yield 2.2 %5 mm/min; ASTM D638
 2.3 %5 mm/min; ISO 527
Tensile Modulus 4740 MPa1 mm/min; ISO 527
 5200 MPa50 mm/min; ASTM D638
Flexural Strength 103 MPaISO 178
 120 MPabrk, 1.3 mm/min, 50 mm span; ASTM D790
 121 MPayld, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 4250 MPa1.3 mm/min, 50 mm span; ASTM D790
 4250 MPa2 mm/min; ISO 178
Izod Impact Notched 95.0 JASTM D256
Izod Impact, Unnotched 700 J/mASTM D4812
Izod Impact, Notched (ISO) 9.00 kJ/m²80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 44.0 kJ/m²80*10*4; ISO 180/1U
Dart Drop, Total Energy 10.0 JASTM D3763
Impact Test 2.00 JMultiaxial Impact; ISO 6603
 
Electrical PropertiesOriginal ValueComments
Surface Resistance 1.00e+9 - 1.00e+11 ohmASTM D257
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 31.0 µm/m-°C
@Temperature -30.0 - 30.0 °C
ASTM D696
CTE, linear, Transverse to Flow 137 µm/m-°C
@Temperature -30.0 - 30.0 °C
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 204 °CFlatw 80*10*4 sp=64mm; ISO 75/Bf
 207 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 181 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 185 °C
@Thickness 3.20 mm
unannealed; ASTM D648
 
Processing PropertiesOriginal ValueComments
Zone 2 265 - 275 °C
Zone 3 275 - 290 °C
Melt Temperature 265 - 275 °CInjection Molding
Mold Temperature 80.0 - 95.0 °C
Drying Temperature 80.0 °CInjection Molding
Dry Time 4.00 hourInjection Molding
Back Pressure 0.300 - 0.700 MPa
Screw Speed 30 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH81425 / 289372

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.