MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Universal Wire Works E91T1-B3 Flux Cored Carbon Steel Tubular Electrode
Categories: Metal; Ferrous Metal; Carbon Steel

Material Notes: Alloy 91T1-B3 is a low alloy steel electrode for single and multiple pass welding of 2.25% chromium, 1 % molybdenum high temperature creep resistant steels in all positions. The fast freezing slag system provides high welder appeal and easy removal. This alloy is formulated for welding ASTM A387 Gr. 22 plate and A335 P22 pipe steels. Extensively used in the fabrication of pressure vessels, boilers, heat exchangers and other applications involved with high temperature exposure and creep resistance.

Shielding Gas: 100% CO2 @ 35-50 cfh

Information provided by Universal Wire Works for their line of welding wire and filler metal.

Key Words: AWS A5.29 E91T1-B3; ASME SFA-5.29 E91T1-B3
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 107000 psipost-weld heat-treated
Tensile Strength, Yield 97200 psi
Elongation at Break 17 %
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.060 %
Chromium, Cr 2.32 %
Iron, Fe 95.2 %As Remainder
Manganese, Mn 0.97 %
Molybdenum, Mo 1.11 %
Phosphorus, P 0.013 %
Silicon, Si 0.32 %
Sulfur, S 0.017 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Mitsui Arlen™ A335 35% Glass Fiber-Reinforced Modified Nylon 6T (DAM)
321 Stainless Steel, annealed sheet
Universal Wire Works E81T1-B2 Flux Cored Carbon Steel Tubular Electrode
TIMET TIMETAL® 1100 Titanium Alloy (Ti-6Al-2.7Sn-4Zr-0.4Mo-0.45Si), Beta Anneal + 1400°F
TIMET TIMETAL® 15-3 Titanium Alloy (Ti-15V-3Cr-3Sn-3Al), Anneal Strip/Sheet

NUWW174 / 19673

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.