MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
DuPont Mobility and Materials BETASEAL™ 1869 Adhesive
Categories: Polymer; Adhesive; Thermoset

Material Notes: Warm processable, high viscosity, high modulus, low conductive glass bonding adhesive can be used primerless on paint.

Information provided by DuPont Performance Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.27 - 1.37 g/ccISO 845
Solids Content >= 97 %
Viscosity Measurement 50 - 100
@Thickness 4.00 mm,
Temperature 55.0 °C
g/min Extrusion Viscosity; 4bar
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 65 - 82DIN 53505
Elongation at Break 7.0 %ISO 1798
 150 %ISO 1798
Stiffness Modulus 0.00250 - 0.00350 GPa
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+9 ohm-cm
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 100 °CTemperature stability
Minimum Service Temperature, Air -40.0 °CTemperature stability
 
Processing PropertiesOriginal ValueComments
Processing Temperature 60.0 - 70.0 °C
Shelf Life 6.00 Month
@Temperature 5.00 - 25.0 °C
unopened containers
 
Descriptive Properties
BasisPolyurethane prepolymers
ColorBlack
CompatibilityGlass
 Paint
Cure rate3 mmafter 24h
PolymerAdhesive
Regional AvailabilityAsia Pacific
 Europe
 Near East/Africa
Sagging30°On vertical wall tilting (maximum)
Skinning time8 to 20

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDTF9179c / 295960

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.