MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
3M Dyneon™ PFE 133TB High Temperature Perfluoroelastomer
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer

Material Notes: 3M™ Dyneon™ PFE 133TBZ is a technically advanced high temperature perfluorelastomer (HT PFE). It is designed to meet the challenges of higher temperature plasma applications. It is classified as FFKM per ASTM D1418. Its fully fluorinated backbone structure provides a very broad chemical and thermal stability

Features and Benefits:

  • Upper use temperature of 315°C
  • Excellent compression set resistance offering enhanced sealing force retention and seal life
  • Ideal for dry side (thermal processes) semiconductor applications including plasma
  • Low metal ion content with low extractables

Information provided by 3M

Key Words: Formerly PFE 133TBZ
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.00 g/cc
Mooney Viscosity 110
@Temperature 121 °C
ML (1+10)
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 79Press Cure 15 Minutes @ 188°C (370°F), Post Cure 24 Hours @ 250°C (482°F); ASTM D2240
Tensile Strength at Break 16.0 MPaPress Cure 15 Minutes @ 188°C (370°F), Post Cure 24 Hours @ 250°C (482°F)
Elongation at Break 192 %Press Cure 15 Minutes @ 188°C (370°F), Post Cure 24 Hours @ 250°C (482°F)
100% Modulus 0.00910 GPa
@Strain 100 %
Press Cure 15 Minutes @ 188°C (370°F), Post Cure 24 Hours @ 250°C (482°F)
Compression Set 26 %
@Temperature 232 °C,
Time 252000 sec
-214 O-rings, 25% Deformation; ASTM D395 Method B
 39 %
@Temperature 232 °C,
Time 605000 sec
-214 O-rings, 25% Deformation; ASTM D395 Method B
 60 %
@Temperature 300 °C,
Time 252000 sec
-214 O-rings, 25% Deformation; ASTM D395 Method B
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 315 °C
Brittleness Temperature -35.0 °C
Transformation Temperature -2.00 °CTR 10
 
Descriptive Properties
ColorWhite
FormCrumb
MH, Maximum Torque15.5 In-lb100 cpm, 0.5° Arc, 15 Minutes @ 188°C (370°F), ASTM D5289
ML, Minimum Torque1.5 In-lb100 cpm, 0.5° Arc, 15 Minutes @ 188°C (370°F), ASTM D5289
t’50, Time to 50% Cure2.7 minutes100 cpm, 0.5° Arc, 15 Minutes @ 188°C (370°F), ASTM D5289
t’90, Time to 90% Cure5.8 minutes100 cpm, 0.5° Arc, 15 Minutes @ 188°C (370°F), ASTM D5289
ts2, Time to 2 Inch-lb Rise from Minimum1.8 minutes100 cpm, 0.5° Arc, 15 Minutes @ 188°C (370°F), ASTM D5289

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
3M Dyneon™ PFE 300Z Clear Perfluoroelastomer System
3M Dyneon™ PFE 191T High Temperature Perfluoroelastomer
Saint-Gobain Fluoroloy® A15 High Performance Seal Material
Seals Eastern 5717 Fluorocarbon-Elastomer
3M Dyneon™ PFE 132TB High Temperature Perfluoroelastomer

PMM33045 / 167792

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.