Bonding: PP, PE Typical Applications: Antena; Exhaust duct; Window seal; Fender Material Advantages: Excellent compression set; Excellent oil resistance; Good weather resistance; Excellent resistance against UV light tested per ASTM G154; Good heat resistance; Good chemical resistance Information provided by Everlon TPE/TPR Manufacturing Experts |