MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Parker Chomerics WIN-SHIELD™ Elite EMI Shielded Window
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Optical Grade

Material Notes: Description: Shielded Windows WIN-SHIELD™ Elite EMI shielded windows provide exceptional optical performance without sacrificing EMI shielding. This new generation of shielded windows is designed specifically to address shielding concerns in electronic equipment such as medical devices, industrial process, measurement and control equipment, and test equipment. WIN-SHIELD™ Elite windows use a proprietary mesh shielding design that provides superior light transmission and EMI shielding properties when compared to traditional shielded window designs. Total shielded window light transmittance properties; result from the mesh, substrates and surface finishes used. This new design also minimizes the typical problem with text distortion on display screens caused by the shielding mesh orientation, i.e., the moiré effect. WIN-SHIELD™ Elite EMI shielded windows are manufactured as a fully laminated construction with optically matched adhesives and front and rear UL HB rated, optical grade, polycarbonate substrates

Information provided by Chomerics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Thickness 1200 - 1800 micronsStandard
 1700 - 2300 micronsStandard
 2700 - 3300 micronsStandard
 3700 - 4300 micronsStandard
 
Electrical PropertiesOriginal ValueComments
Shielding Effectiveness 35 dB
@Frequency 1e+10 Hz
14" x 14" open aperture; MIL-STD-285; CHO-TM-TPO8
 55 dB
@Frequency 1e+9 Hz
14" x 14" open aperture; MIL-STD-285; CHO-TM-TPO8
 57 dB
@Frequency 2.00e+9 Hz
14" x 14" open aperture; MIL-STD-285; CHO-TM-TPO8
 67 dB
@Frequency 1e+8 Hz
14" x 14" open aperture; MIL-STD-285; CHO-TM-TPO8
 73 dB
@Frequency 2.00e+8 Hz
14" x 14" open aperture; MIL-STD-285; CHO-TM-TPO8
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 70.0 °C
Minimum Service Temperature, Air -40.0 °C
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 75 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Parker Chomerics CHO-FORM 5526 EMI Shielding Material
Parker Chomerics POLASHEET® Metal EMI Gasket
Parker Chomerics MESH STRIP™ (Elastomer Core) Wire Mesh EMI Gasket Selection Guide
Parker Chomerics CHO-VER SHIELD™ EMI Shielding Covers with Over-Molded Conductive Elastomer Gasket
Parker Chomerics CHO-FORM 5532 EMI Shielding Material

PCHOME285 / 130995

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.