MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
KLJ Group KANATOL FLAMEGUARD C 100 Phosphate Esters
Categories: Fluid

Material Notes: Properties: TCP-100 is general purpose tri aryl phosphate. It is colourless to pale yellow liquid free of foreign materials. It is widely used among Phosphoric Ester due to its characteristic like fire retardancy, electrical insulation, low volatility and insolubility in water.

Application: TCP-100 is used in flexible PVC, cellulose nitrate and ethyl cellulose coating. TCP-100 is used in electrical cable compound for FR properties and also in synthetic compound. It has low volatility, good saponification resistance and good resistance to extraction by oil hence used as a lubricants adhesives for extreme pressure and fire risk from heat source and electrical sparks. TCP-100 is used in vinyl tarpaulin, conveyer belts air ducks etc.

Chemical Name: TRI CRESYL PHOSPHATE (TCP)

Molecular Formula: C 21 H21 O 4 P

CAS Number: 1330-78-5

UN. NO.: 3082

EINECS NO.: 215-548-8

Information provided by KLJ Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.169 - 1.171 g/ccASTM D1045-08
Brookfield Viscosity 55 - 70 cPASTM D445
Molecular Weight 368.37 g/mol
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.55 - 1.566
@Temperature 27.0 °C
ASTM D1045-08
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 0.10 %ASTM E203-01
 
Component Elements PropertiesOriginal ValueComments
Phosphorus, P 8.4 - 8.5 %KLJ/QCD/WIN/49
 
Descriptive Properties
Acidity as H3PO4<0.01%ASTM D1613
AppearanceClear Liquid
Color<150Hazen, ASTM D1045-86
Content<0.05%Free Alcohol, KLJ/QCD/WIN/46
 <0.5%O-Isomer Content, GLC KLJ/QCD/WIN/50
 <10 ppmWater Soluble Impurities, BS-1998:1970
 >99%Ester Content, GLC KLJ/QCD/WIN/50
 >99%Cresolic Ester Content, GLC KLJ/QCD/WIN/50

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PKLJ260 / 284281

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.