MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Borealis Bormed™ LE6603-PH LDPE for Healthcare Applications  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Molded

Material Notes: Bormed LE6603-PH is a low density polyethylene for injection molding having excellent flow properties allowing short cycle time or easy filling of long flow-paths. The molded article is characterized by low degree of built-in stress and good flexibility.

Bormed LE6603-PH is recommended for injection molding of flexible lids, caps and closures, and pharmaceutical and diagnostic packaging.

Information provided by the Manufacturer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.923 g/ccISO 1183
Melt Flow 22 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 49ISO 868
Elongation at Break 130 %ISO 527-2
Tensile Modulus 0.180 GPaISO 527-2
Tensile Impact Strength 160 kJ/m²ISO 8256/A1
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 92.0 °CISO 306
 
Processing PropertiesOriginal ValueComments
Melt Temperature 180 - 230 °C
Mold Temperature 10.0 - 40.0 °C

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Braskem PB 608 LDPE Injection Molding Polyethylene
Braskem PB 208 LDPE Injection Molding Polyethylene
Braskem G803 LDPE Injection Molding Polyethylene
Braskem F7018 LDPE Injection Molding Polyethylene
Braskem BI 818 LDPE Injection Molding Polyethylene

PBOREA077 / 216140

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.