MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Lubrizol Pearlbond™ 223 Polyurethane
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Pearlbond® 223 is a linear, polycaprolactone-based polyurethane, supplied in form of small white granules, which combines an extremely high crystallization rate with a very high thermoplasticity level. It is used for Hot Melt adhesives.

Information provided by The 159 Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.19 g/ccISO 2781
Viscosity 650 cP
@Load 2.16 kg,
Temperature 160 °C
ISO 1133
Melt Flow 60 - 100 g/10 min
@Load 2.16 kg,
Temperature 170 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 54ISO 868
 
Thermal PropertiesOriginal ValueComments
Melting Point 64.0 - 68.0 °CMQSA 70A
Softening Point 55.0 - 60.0 °CMQSA 70A
 
Processing PropertiesOriginal ValueComments
Zone 1 100 - 110 °C
Zone 2 120 - 130 °C
Zone 3 125 - 135 °C
Zone 4 125 - 135 °C
Die Temperature 135 - 145 °C
Screw Speed 40 - 50 rpm
 
Descriptive Properties
Crystallization rateVery HighMQSA 12A
ThermoplasticityVery HighMQSA 68A

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLUBR5036 / 238906

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.