MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Ascend Performance Materials Vydyne® AST03 PA66-I
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Impact Grade

Material Notes: Vydyne AST03 is an impact modified PA66 resin for injection molded applications.

Information provided by Ascend Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.08 g/ccDAM; ISO 1183
Moisture Absorption at Equilibrium 1.6 %DAM to 50% RH; ISO 62
Water Absorption at Saturation 6.0 %ISO 62
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 65.0 MPaDAM; ISO 527-2
Elongation at Break 60 %DAM; ISO 527-2
Elongation at Yield 4.6 %DAM; ISO 527-2
Tensile Modulus 2500 MPaDAM; ISO 527-2
Flexural Strength 90.0 MPaDAM; ISO 178
Flexural Modulus 2700 MPaDAM; ISO 178
Izod Impact, Notched (ISO) 35.0 kJ/m²
@Temperature -40.0 °C
DAM; ISO 180/1A
 55.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 180/1A
Charpy Impact Unnotched 100 kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eU
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+16 ohm-cm
@Thickness 1.00 mm
DAM; IEC 60093
Comparative Tracking Index 600 V
@Thickness 3.00 mm
IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 95.0 µm/m-°C
@Thickness 2.00 mm,
Temperature 35.0 - 55.0 °C
DAM; ISO 11359-2
CTE, linear, Transverse to Flow 125 µm/m-°C
@Thickness 2.00 mm,
Temperature 23.0 - 55.0 °C
DAM; ISO 11359-2
UL RTI, Electrical 65.0 °C
@Thickness 0.750 mm
UL 746
 65.0 °C
@Thickness 1.50 mm
UL 746
 65.0 °C
@Thickness 3.00 mm
UL 746
UL RTI, Mechanical with Impact 65.0 °C
@Thickness 0.750 mm
UL 746
 65.0 °C
@Thickness 1.50 mm
UL 746
 65.0 °C
@Thickness 3.00 mm
UL 746
UL RTI, Mechanical without Impact 65.0 °C
@Thickness 0.750 mm
UL 746
 65.0 °C
@Thickness 1.50 mm
UL 746
 65.0 °C
@Thickness 3.00 mm
UL 746
Flammability, UL94 HB
@Thickness 0.750 mm
 HB
@Thickness 1.50 mm
 HB
@Thickness 3.00 mm
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 250 - 260 °CInjection
Middle Barrel Temperature 265 - 275 °CInjection
Front Barrel Temperature 265 - 275 °CInjection
Melt Temperature 265 - 275 °CInjection
Mold Temperature 60.0 - 80.0 °CInjection
Drying Temperature 75.0 - 85.0 °CInjection
Dry Time 4.00 hourInjection
Moisture Content 0.20 %Injection
 
Descriptive Properties
AdditiveRelease agent
Agency RatingsISO, 1043 PA66 I
AppearanceNatural Color
FeaturesImpact Modified
FormsPellets
Processing MethodInjection Molding
RegionNorth America, Europe

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PASCE8520 / 296324

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.