MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SAE 980X HSLA Steel
Categories: Metal; Ferrous Metal; Alloy Steel; Low Alloy Steel

Material Notes: Higher strength but lower formability than 945X and 950X.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.75 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate >= 655 MPa
Tensile Strength, Yield >= 550 MPa
@Strain 0.2 %
Elongation at Break 10 %
Modulus of Elasticity 206 GPa
Bulk Modulus 163 GPaEstimated from elastic modulus
Poissons Ratio 0.29Typical for steel
Shear Modulus 80.0 GPaEstimated from elastic modulus

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ASTM A284 Steel, grade C
SAE 960X HSLA Steel
ArcelorMittal HSLA 550 High strength low alloy steel for cold forming, Hot Rolled
SAE 950X HSLA Steel
ASTM A812 HSLA Steel Grade 80 Sheet

MSSAE980X / 100266

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.