MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
LG Chemical LUMAX GP5200B PBT+ABS+GF20%
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled

Material Notes: Description: Injection Molding Grade, PBT+ABS+GF20%, General Purpose

Application: E&E (Speaker Frame)

CAS: 9003-56-9, 65997-17-3, 24968-12-5 and 9003-54-7

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.35 g/ccASTM D792
Maximum Moisture Content 0.020Injection Molding
Linear Mold Shrinkage, Flow 0.0040 - 0.0090 cm/cm
@Thickness 3.20 mm
ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 950 kg(f)/cm²
@Thickness 3.20 mm
5mm/min; ASTM D638
Elongation at Break 3.0 %
@Thickness 3.20 mm
5mm/min; ASTM D638
Flexural Yield Strength 1450 kg(f)/cm²
@Thickness 3.20 mm
1.3mm/min; ASTM D790
Flexural Modulus 58000 kg(f)/cm²
@Thickness 3.20 mm
1.3mm/min; ASTM D790
Izod Impact, Notched 6.50 kg-cm/cm
@Thickness 3.20 mm,
Temperature 23.0 °C
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Melting Point 225 °CPeak at Break
Deflection Temperature at 0.46 MPa (66 psi) 195 °C
@Thickness 6.40 mm
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 160 °C
@Thickness 6.40 mm
Unannealed; ASTM D648
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 225 - 235 °CInjection Molding
Middle Barrel Temperature 230 - 245 °CInjection Molding
Front Barrel Temperature 240 - 250 °CInjection Molding
Nozzle Temperature 240 - 250 °CInjection Molding
Melt Temperature 240 - 250 °CInjection Molding
Mold Temperature 60.0 - 80.0 °CInjection Molding
Drying Temperature 100 °CInjection Molding
Dry Time 4.00 - 5.00 hourInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LG Chemical LUPOS GP2100 ABS+GF10%, General Purpose
LG Chemical LUPOS GP2200 ABS+GF20%, General Purpose
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 10% Glass Fiber Filled
Overview of materials for Polycarbonate/ABS Alloy, Glass Fiber Filled
LG Chemical LUPOS GP2300 ABS+GF30%, General Purpose

PLAY452 / 148462

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.