Impact modified acrylic resin, injection molding grade Applications: A high flow, impact-modified acrylic resin designed for medical or food uses. This resin offers impact strengths up to seven times of general-purpose acrylic resins and is suited for Gamma irradiation treatment. Meets FDA CFR-21 Sec 177.1010 for food use. Meets USP Plastic Class VI for medical use. UV transmitting. |