MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ExxonMobil Santoprene® 8221-70 Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes: A soft, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range of applications. This grade of Santoprene TPV is shear-dependent and can be processed on conventional thermoplastics equipment for injection molding or blow molding. It is polyolefin based and completely recyclable.

Key Features:

  • UL listed: file #QMFZ2.E80017, Plastics - Component; file #QMFZ8.E80017, Plastics Certified For Canada - Component.
  • Neutral, easy coloring formulation.
  • Used in sealing applications.
  • EU and China RoHS compliant.
Applications:
  • Industrial – Architecture and Construction
Uses:
  • Construction Applications
  • Expansion Joint
  • Glazing
  • Outdoor Applications
Processing Method: Blow Molding, Extrusion Blow Molding, Injection Blow Molding, Injection Molding and Multi Injection Molding

Availability: Africa & Middle East, Europe, North America, Asia Pacific, Latin America and South America

Information provided by ExxonMobil Chemical

Key Words: EU 2003/11/EC; RoHS Compliant; UL QMFZ2; UL QMFZ8
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.950 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 752 mm, 15 sec; ISO 868
Tensile Strength at Break 986 psiAcross Flow; ASTM D412
Tensile Stress at Strain 421 psi
@Strain 100 %
Across Flow; ASTM D412
Elongation at Break 600 %Across Flow; ASTM D412
Tear Strength 143 pli73°C, Die C; ASTM D624
Compression Set 38 %
@Temperature 70.0 °C,
Time 79200 sec
ASTM D395
 58 %
@Temperature 125 °C,
Time 252000 sec
ASTM D395
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature -80.0 °FASTM D746
UL RTI, Electrical 100 °CUL 746
UL RTI, Mechanical with Impact 85.0 °CUL 746
Flammability, UL94 HB
@Thickness 1.10 mm
 HB
@Thickness 1.60 mm
 HB
@Thickness 3.00 mm
 
Processing PropertiesOriginal ValueComments
Processing Temperature 175 - 230 °C
Rear Barrel Temperature 355 - 385 °F
Middle Barrel Temperature 365 - 390 °F
Front Barrel Temperature 375 - 400 °F
Nozzle Temperature 375 - 410 °F
Die Temperature 365 - 430 °FExtrusion
Melt Temperature 365 - 430 °FExtrusion
 390 - 420 °FProcessing
Mold Temperature 75.0 - 125 °FProcessing
Moisture Content 0.080 %
Back Pressure 50.0 - 100 psi
Clamp Pressure 6000 - 10000 psi
Vent Depth 0.00100 in
Cushion 0.125 - 0.250 in
Screw Speed 100 - 200 rpm
 
Descriptive Properties
ColorNatural Color
FormPellets
Injection RateFast
Maximum Regrind %20
Screw Compression Ratio2:1 - 2.5:1
Screw L/D Ratio16:1 - 20:1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ExxonMobil Santoprene® 8221-75M300 Thermoplastic Elastomer
ExxonMobil Santoprene® 8221-85M300 Thermoplastic Elastomer
ExxonMobil Santoprene® 8201-70 Thermoplastic Elastomer
ExxonMobil Santoprene® 8201-60 Thermoplastic Elastomer
ExxonMobil Santoprene® 8271-55 Thermoplastic Elastomer

PADVA018 / 22708

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.