Product Description: Exceed 4518 resins are metallocene ethylene-hexene copolymer. Films made from Exceed 4518 have outstanding tensile properties and impact and puncture toughness. These superior properties together with excellent drawability, make this a versatile polymer for mono layer and multilayer packaging and cast stretch film. Availability: Latin America, North America and South America Additive: - Antiblock: No
- Slip: No
- Processing Aid: No
- Thermal Stabilizer: Yes
Applications: - Cast Film
- Cast Stretch Film
- Diaper Backsheet
- Hygiene Film
- Packaging Film
- Personal Care
Information provided by ExxonMobil |