MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) KetaSpire® XT-920 PEEK
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK)

Material Notes: KetaSpire® XT-920 is an unreinforced, natural color grade of the industry's first true high-temperature PEEK polymer supplied in a lubricated pellet form. The PEEK designation is based on the 2:1 ratio of ether-to-ketone functional groups in the polymer backbone.

The material provides the exceptional chemical resistance of PEEK along with a 20°C (36°F) higher glass transition temperature and a 45°C (81°F) higher melting temperature than standard PEEK. This increase in thermal performance allows engineers to achieve higher mechanical strength for components used in higher temperature and higher pressure operating environments. KetaSpire® XT also provides a significant improvement in electrical properties.

Although other high-temperature polyketones exhibit thermal properties on par with KetaSpire® XT, their chemical resistance is significantly inferior to standard PEEK and KetaSpire® XT. The material's unique combination of properties makes KetaSpire® XT well-suited for applications in oil & gas, transportation, electronics, chemical processing, and other industrial uses. KetaSpire® XT-920 can be easily processed using typical injection molding and extrusion processes. This resin is also available as KetaSpire® XT-920P in a natural-color coarse powder form for compounding.

Pellets of KetaSpire® XT-920 are supplied lightly dusted with the lubricant calcium stearate (0.01% level) to aid with pellet conveyance in plastication screws. The equivalent non-lubricated, natural color grade is KetaSpire® XT-920 NL.

- Natural: XT-920 NT

Applications: Aircraft Applications; Automotive Applications; Communication Wire Insulation; Connectors; Electrical/Electronic Applications; Film; Gears; Housings; Industrial Applications; Oil/Gas Applications; Pump Parts; Seals; Tubing

Features: Chemical Resistant; Ductile; Fatigue Resistant; Flame Retardant; Good Dimensional Stability; Good Impact Resistance; High Heat Resistance; Radiotranslucent; Steam Resistant

Injection notes: Drying
- KetaSpire® XT resins must be dried completely prior to melt processing. Incomplete drying will result in defects in the formed part ranging from surface streaks to severe bubbling. Pellets can be dried on trays in a circulating air oven or in desiccating hopper dryer. Drying conditions recommended are 4 hours at 150°C (300°F) .
Injection Molding
- KetaSpire® XT resins can be readily injection molded in most screw injection machines. A general purpose screw with a compression ratio in the range of 2.5 - 3.5 : 1 is recommended, as is minimum back pressure. Injection speeds should be as fast as possible, consistent with part appearance requirements. Mold temperatures in the range of 205°C to 230°C (400°F to 450°F) are suggested. Recommended starting point barrel temperatures are shown in the table above.

Information provided by Solvay Specialty Polymers.

Vendors: Drake extrudes shapes and machines and injection molds parts in Torlon® PAI, PEEK, PAEK, Ryton PPS and Ultem PEI. It also machines Vespel® PI. Innovations include cryogenic CryoDyn® CT-200 shapes as a PCTFE alternative; efficient Seamless Tube® and the largest extruded rod diameters to >254mm and plate thicknesses to > 100mm. Certified to ISO 9001:2015 and AS9100D. Visit www.DrakePlastics.com

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.28 g/ccASTM D792
Water Absorption 0.090 %
@Time 86400 sec
ASTM D570
Viscosity 410 cP
@Shear Rate 1000 1/s,
Temperature 420 °C
Melt; ASTM D3835
Linear Mold Shrinkage, Flow 0.011 - 0.013 cm/cm
@Thickness 2.00 mm
ASTM D955
Linear Mold Shrinkage, Transverse 0.015 - 0.017 cm/cm
@Thickness 2.00 mm
ASTM D955
Melt Flow 9.7 g/10 min
@Load 2.16 kg,
Temperature 420 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 91ASTM D785
Hardness, Shore D 86
@Time 1.00 sec
ASTM D2240
Tensile Strength 93.0 MPa50 mm/min; ASTM D638
Tensile Strength, Yield 93.0 MPaType 1A, 50 mm/min; ISO 527-2
Elongation at Break 28 %50 mm/min; ASTM D638
Elongation at Yield 6.1 %Type 1A, 50 mm/min; ISO 527-2
 6.4 %50 mm/min; ASTM D638
Tensile Modulus 3400 MPa1 mm/min, Type 1A; ISO 527-2
 3400 MPa50 mm/min; ASTM D638
Flexural Strength 106 MPaISO 178
 135 MPaASTM D790
Flexural Modulus 3300 MPaISO 178
 3600 MPaASTM D790
Compressive Strength 114 MPaASTM D695
Poissons Ratio 0.41ASTM E132
Shear Strength 89.0 MPaASTM D732
Izod Impact, Notched 100 J/mASTM D256
Izod Impact, Unnotched NBASTM D256
Izod Impact, Notched (ISO) 9.00 kJ/m²ISO 180
Izod Impact, Unnotched (ISO) NBISO 180
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 3.1
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 23.0 kV/mm
@Thickness 1.60 mm
ASTM D149
Dissipation Factor 0.0026
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 44.0 µm/m-°C
@Temperature -50.0 - 50.0 °C
ASTM E831
Melting Point 385 °CPeak; ASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 175 °C
@Thickness 3.20 mm
Annealed; ASTM D648
Glass Transition Temp, Tg 170 °CDSC
Flammability, UL94 V-0
@Thickness 0.800 mm
 V-0
@Thickness 1.60 mm
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 395 °C
Middle Barrel Temperature 395 °C
Front Barrel Temperature 405 °C
Nozzle Temperature 405 °C
Mold Temperature 205 - 230 °C
Drying Temperature 150 °C
@Time 14400 sec
 
Descriptive Properties
AdditiveLubricant
AvailabilityAsia Pacific
 Europe
 North America
ColorBeige
FormsPellets; Powder
Injection RateFast
ProcessingFilm Extrusion; Injection Molding; Machining; Profile Extrusion; Wire & Cable Extrusion
RoHS ComplianceYes
Screw Compression Ratio2.5:1.0 to 3.5:1.0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSOL8Y4351 / 280151

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.