MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
FKuR Kunststoff Fibronlon® S 7530 Wood-Plastic Composite
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic

Material Notes: Fibrolon® S 7530 is a biodegradable compound with a high content of natural resources. This grade is predominantly used for injection molding. Processing in profile extrusion is also possible. Natural fiber reinforced compound for injection molding made from renewable resources.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.27 g/ccISO 1183
Melt Flow 9.0 - 11 g/10 min
@Load 5.00 kg,
Temperature 190 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 36.5 MPaISO 527
Tensile Strength, Ultimate 36.5 MPaISO 527
Tensile Strength, Yield 37.0 MPaISO 527
Tensile Modulus 3850 MPaISO 527
Flexural Modulus 3650 MPaISO 178
Flexural Strain at Break 2.8 %ISO 178
Charpy Impact Unnotched 8.00 kJ/m²
@Temperature 23.0 °C
ISO 179-1/1 eU
Charpy Impact, Notched 3.70 kJ/m²ISO 179-1/1 eA
 
Thermal PropertiesOriginal ValueComments
Melting Point 140 - 160 °CISO 3146-C
Vicat Softening Point 105 °CISO 306
 
Descriptive Properties
Bio-based carbon content (%)75ASTM D 6866

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
FKuR Kunststoff Fibrolon® F 8530 Biodegradable Wood-Plastic Compound, Fiber Reinforced
FKuR Kunststoff Fibronlon® P 8540 Wood-Plastic Composite
FKuR Kunststoff Fibrolon® P 7550 Wood-Plastic Compound, Fiber Reinforced
FKuR Kunststoff Fibrolon® P 8540 Wood-Plastic Compound, Fiber Reinforced
Overview of materials for Low Density Polyethylene (LDPE), Masterbatch Grade

PFKUR908 / 192729

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.