Uniplex FRX 44-94 S is a powdery flame retardant. The nitrogen and phosphorus blend components form an intumescent layer under heat and fire exposure. It is used as an intumescent flame retardant in thermosets, polyolefin compounds as well as in paints and coatings. Uniplex FRX 44-94 S offers an excellent UV stability. In addition the product is non-hydroscopic. It can be processed at temperatures up to 225°C. Chemical name: Nitrogen and phosphorus containing blend Information provided by Lanxess. |