MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Socomore Aeroglaze® 9924V Wash Primer
Categories: Fluid

Material Notes: Aeroglaze® 9924V wash primer was designed for priming metal surfaces. It is particularly useful for priming non-ferrous substrates such as aluminum and galvanized steel.

Socomore acquired the Aeroglaze® and Chemglaze® product lines from Lord in September 2016.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.850 g/cc9924V; ASTM D1475-85
 0.960 g/ccMixed; ASTM D1475-85
 1.10 g/cc9924A; ASTM D1475-85
Solids Content 0.00 %9924V; by weight; ASTM D2369-87 Modified
 11 %Mixed; by volume; ASTM D2369-87 Modified
 18.2 %Mixed; by weight; ASTM D2369-87 Modified
 33 %9924A; by weight; ASTM D2369-87 Modified
Volatile Organic Compounds (VOC) Content 679 g/l9924A; ASTM D3960-87
 773 g/lMixed; ASTM D3960-87
 830 g/l9924V; ASTM D3960-87
Brookfield Viscosity 225 cPMixed; ASTM D2196-66; LVT, Spindle #3 @ 12rpm
 3000 cP9924A; ASTM D2196-66; LVT, Spindle #3 @ 12rpm
 10 cP
@Temperature 25.0 °C
9924V; ASTM D2196-66; LVT, Spindle #1 @ 60rpm
Viscosity Measurement 11 - 15seconds; Zahn, #4 cup
 48 - 52seconds; Zahn, #2 cup
 
Mechanical PropertiesOriginal ValueComments
Gardner Impact 160 in-lbDirect
 160 in-lbReverse
 
Thermal PropertiesOriginal ValueComments
Flash Point 19.0 °C9924A; Setaflash, Closed Cup; ASTM D3278-82
 20.6 °C9924V; Setaflash, Closed Cup; ASTM D3278-82
 
Processing PropertiesOriginal ValueComments
Dry Time 0.33 hour
@Temperature 22.2 °C
Set to touch; Gardner, Mechanical
 1 hour
@Temperature 22.2 °C
Surface Dry; Gardner, Mechanical
 2 hour
@Temperature 22.2 °C
Dry Hard; Gardner, Mechanical
Pot Life 480 min
Shelf Life 12.0 Month9924V
 6.00 Month
@Temperature <=26.7 °C
9924A
 
Descriptive Properties
AppearanceClear, colorless to straw9924V
 RedMixed
 Red9924A
Conical Mandrel BendPasses 1/8"ASTM D522
Mix Ratio1:1by volume
 8.8:8.8by weight

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLORD120 / 86128

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.