MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
3M AC-215 Class B-2 Aerospace Sealant
Categories: Polymer; Thermoset; Polysulfide Sealant/Adhesive

Material Notes: 3M Aerospace Sealant AC-215 Class B are two-part, polysulfide access door sealants for faying surfaces where easy separation of jointed surfaces is required. They are a highly thixotropic reddish past which can easily be applied with a spatula, putty knife or caulking gun. The cured 3M AC-215 Class B Sealants have low adhesion and form a tough, “rubbery” gasket that molds well to surface irregularities.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.52 g/ccMIL-S-8784
Volatiles 2.0 %
Brookfield Viscosity 700000 - 900000 cPBase, RVF #7 sp @ 2 rpm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 45MIL-S-8784
Peel Strength 2.00 pliAdhesion to Aluminum, steel, stainless steel, titanium, zinc, cadmium, chromium, magnesium, glass, enamel, Epoxy MIL-P-23377 and Urethane MIL-C-27725
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 121 °CMIL-S-8784
Minimum Service Temperature, Air -54.0 °CMIL-S-8784
 
Processing PropertiesOriginal ValueComments
Cure Time 48.0 hour
Tack-Free Time 24.0 hour
 
Descriptive Properties
AppearanceBlackAccelerator
 Red/PinkBase
 Red/Purple

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMM35411 / 170158

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.