Product Description: HD 7925.30 is a medium molecular weight HDPE homopolymer for use in blown and cast film applications. Typical applications include those with low WVTR and clarity requirements. Availability: Latin America, North America and South America Additive: - Antiblock: No
- Slip: No
- Thermal Stabilizer: Yes
Applications: - Barrier Food Packaging
- Blown Film
- Food packaging
- Heavy Duty Bags
- Oriented Film Products
- Skin Layer for OPP
- Stand Up Pouches
Information provided by ExxonMobil Chemical |