MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
ASTM A387 Alloy Steel, Grade 91  (discontinued **)
Categories: Metal; Ferrous Metal; Alloy Steel; Medium Alloy Steel; ASTM Steel; Carbon Steel; Low Carbon Steel

Material Notes: Cr-Mo alloy steel plate
High service temperature

Pressure vessel quality

Spec discontinued in 1989

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.80 g/ccTypical of ASTM Steel
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 585 - 760 MPa
Tensile Strength, Yield 415 MPa
Elongation at Break 18 %in 50mm
Modulus of Elasticity 200 GPaTypical Carbon Steel
Bulk Modulus 160 GPaTypical for Steel
Poissons Ratio 0.29Typical Carbon Steel
Shear Modulus 80.0 GPaTypical for Steel
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000170 ohm-cmTypical Carbon Steel
 
Thermal PropertiesOriginal ValueComments
CTE, linear 12.0 µm/m-°CTypical Carbon Steel
Specific Heat Capacity 0.470 J/g-°CTypical Carbon Steel
Thermal Conductivity 52.0 W/m-KTypical Carbon Steel
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 0.040 %
Carbon, C 0.080 - 0.12 %
Chromium, Cr 8.0 - 9.5 %
Iron, Fe 88.585 %as balance
Manganese, Mn 0.30 - 0.60 %
Molybdenum, Mo 0.85 - 1.05 %
Nickel, Ni 0.40 %
Niobium, Nb (Columbium, Cb) 0.060 - 0.10 %
Nitrogen, N 0.030 - 0.070 %
Phosphorus, P 0.020 %
Silicon, Si 0.20 - 0.50 %
Sulfur, S 0.010 %
Vanadium, V 0.18 - 0.25 %

References for this datasheet.

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ASTM A387 Alloy Steel, Grade 11, Class 1
ASTM A387 Alloy Steel, Grade 11, Class 2
MetalTek MTEK 221-01 Cast UNS J84090 Martensitic Stainless Steel
ASTM A387 Alloy Steel, Grade 9, Class 1
AISI 1009 Steel

MSA38791 / 142849

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.