Availability: Asia Pacific; Europe; North America Fillers/Reinforcement: Mineral, 40% Filler by Weight Automotive Specifications: FORD ESB-M4D353-A2 Color: WT031; FORD WSK-M4D704-A1 Form: Pellets Processing Method: Injection Molding Information provided by Teknor Apex |