MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Solvay Chemicals Polyglycerol-3
Categories: Fluid

Material Notes: A polyglycerol characterized by a very narrow oligomer distribution centered on triglycerol.

EINECS Number: 915-741-3/CAS Number: 25618-55-7

Information provided by Solvay

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.284 g/cc
Viscosity 41000 cPDynamic
Molecular Weight 250 g/mol
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 30
 
Thermal PropertiesOriginal ValueComments
CTE, linear 540 µm/m-°C
@Temperature 20.0 - 40.0 °C
Specific Heat Capacity 2.24 J/g-°C
Thermal Conductivity 0.260 W/m-K
Flash Point 260 °C
Ignition Temperature 400 °CAutoignition
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.491
 
Descriptive Properties
AppearanceYellowish viscous liquid, having almost no odor
Color<250APHA
Composition<1 g/kgWater
 <10%Pentaglycerol
 <100 mg/kgChloride
 <5%Hexaglycerol and higher oligomers
 10-25%Tetraglycerol
 15-30%Diglycerol
 35-55%Triglycerol
Fire point296°C
Heat of dissolution in water-57 j/g

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Elkem (Bluestar Silicones) BLUESIL™ FLD 47 V 3 Polydimethylsiloxanic Fluids
PBI Performance Products S26 Thermal Resistant Polybenzimidazole Solution
Syensqo (Solvay Specialty Polymers) Galden® DET PFPE Fluid
Paratherm Corporation Paratherm™ NF Heat Transfer Fluid
Syensqo (Solvay Specialty Polymers) Galden® D02TS PFPE Fluid

WSOLV155 / 147804

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.