Casting methods recommended for this alloy: Centrifugal and Sand. Applications: Locomotive wearing parts, high-speed low-load bearings. Classified under: High-leaded tin bronzes. ASTM B66 Alloy does not respond to heat treating |
High lead tin bronze, ASTM B66 |