MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Daikin DAI-EL® G-755CBP Fluoroelastomer Copolymer, Bisphenol Curable Grade, 66% Fluorine Content
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer; Rubber or Thermoset Elastomer (TSE)

Material Notes: DAI-EL® G-755CBP is a bisphenol curable, gum copolymer with low Mooney viscosity. It is designed especially for extrusion and calendering, but may be used for molding.

Typical Applications: Tubing, hoses and sheets goods

Rheological Properties MDR 2000:
Temperature: 177°C
Frequency: 100 cpm
Strain: 0.5°
Test time: 6 min

Rheological Properties ODR:
Temperature: 177°C
Frequency: 100 cpm
Strain: 3 °
Test time: 12 min

Information provided by Daikin.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.81 g/cc
Mooney Viscosity 25
@Temperature 121 °C
ML 1+10
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 74ODR
 75MDR 2000
Tensile Strength at Break 13.1 MPaODR
 13.8 MPaMDR 2000
Elongation at Break 210 %MDR 2000
 210 %ODR
100% Modulus 5.40 MPa
@Strain 100 %
MDR 2000
 5.70 MPa
@Strain 100 %
ODR
Compression Set 15 %
@Temperature 200 °C,
Time 252000 sec
#214 O-ring, MDR 2000; ASTM D395 Method B
 20 %
@Temperature 200 °C,
Time 252000 sec
#214 O-ring, ODR; ASTM D395 Method B
 
Thermal PropertiesOriginal ValueComments
Minimum Service Temperature, Air -18.0 °CLow Temperature Retraction; ASTM D1329
 
Processing PropertiesOriginal ValueComments
Cure Time 1.00 mints2, scorch time, MDR 2000
 1.20 mint'50, time to 50% cure, MDR 2000
 1.70 mints2, scorch time, ODR
 1.90 mint'90, time to 90% cure, MDR 2000
 2.50 mint'50, time to 50% cure, ODR
 2.80 mint'90, time to 90% cure, ODR
 5.00 min
@Temperature 177 °C
Press Cure, ODR
 10.0 min
@Temperature 177 °C
Press Cure, MDR 2000
 24.0 hour
@Temperature 232 °C
Post Cure, MDR 2000
 24.0 hour
@Temperature 260 °C
Post Cure, ODR
 
Component Elements PropertiesOriginal ValueComments
Fluorine, F 66 %
 
Descriptive Properties
ColorWhite to pale brown
MH10 dNmmaximum torque, MDR 2000
 108 dNmmaximum torque, ODR
ML1.1 dNmminimum torque, MDR 2000
 10 dNmminimum torque, ODR
Test Formula0.5 phrPhosphonium accelerator
 100 phrDAI-EL® G-755CBP
 2 phrBisphenol AF
 3 phrMagnesium oxide
 30 phrMT Carbon Black (N-990)
 6 phrCalcium hydroxide

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDAIJ9823 / 209894

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.