MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Rogers Arlon 55141R028 Silicone Rubber/Fiberglass Laminate
Categories: Polymer; Thermoset; Silicone; Silicone Rubber; Silicone, Molded, Glass Fiber Filled

Material Notes: Interleave: 3 mil PE; Side 1: uncured silicone rubber; Substrate: 162 fiberglass; Side 2: uncured silicone rubber; Interleave 2: 3 mil PE

Information provided by Arlon Silicone Technologies; now a part of Rogers Corporation.

Key Words: UL Recognition E54153 (200°C/200°C)
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.35 g/ccsilicone property, side 1; Arlon SQA-TMS-024
 1.35 g/ccsilicone property, side 2; Arlon SQA-TMS-024
Thickness 5.00 milside 1; Arlon SQA-TMS-003
 5.00 milside 2; Arlon SQA-TMS-003
 18.0 milsubstrate; Arlon SQA-TMS-003
 28.0 miloverall; Arlon SQA-TMS-003
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 60silicone property, side 1; ASTM D2240
 60silicone property, side 2; ASTM D2240
Tensile Strength, Ultimate 800 psisilicone property, side 1; ASTM D412
 800 psisilicone property, side 2; ASTM D412
Elongation at Break 225 %silicone property, side 1; ASTM D412
 225 %silicone property, side 2; ASTM D412
Adhesive Bond Strength 7.30 psiASTM D624
Tear Strength 90.0 plisilicone property, side 1; ASTM D624
 90.0 plisilicone property, side 2; ASTM D624
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 780 V/milASTM D149
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 450 °F
Minimum Service Temperature, Air -70.0 °F
UL RTI, Electrical 200 °C
UL RTI, Mechanical without Impact 200 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 2.00 hour
@Temperature 204 °C
 15.0 min
@Pressure 0.345 MPa,
Temperature 121 °C
Shelf Life 6.00 Month
@Temperature 23.9 °C
 
Descriptive Properties
ColorRed

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Rogers Arlon 56976XA026 Silicone Rubber/Fiberglass Laminate
Rogers Arlon Thermabond® 99180T010 Silicone Rubber/Fiberglass Laminate
Rogers Arlon 55096R028 Silicone Rubber/Fiberglass Laminate
Overview of materials for Silicone Rubber
Rogers Arlon 51106R015 Silicone Rubber/Fiberglass Laminate

PARL032 / 79684

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.