MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Akrochem Sorbacid® 911 Magnesium Aluminum Hydroxy Carbonate
Categories: Other Engineering Material

Material Notes: Product Description: Sorbacid 911 is a synthetic, fine, white powder used as a lead replacement in halogenated polymers to scavenge acid by-products, which are detrimental to many polymeric processing and physical properties. Chemically, Sorbacid 911 is magnesium aluminum hydroxy carbonate. Sorbacid 911 has the added benefit of releasing water at 300°C (higher than ATH, thus safer processing) and therefore are used as flame-retardants and smoke suppressants. Sorbacid 911 product is environmentally safe, non-toxic, non-corrosive and non-volatile.

Applications: Sorbacid 911 is primarily utilized as a lead oxide (e.g., litharge, red lead, BSWL) replacement to scavenge acidic byproducts in halogenated polymers such as: polychloroprene (CR), chlorosulfonated polyethylene (CSM), chlorinated polyethylene (CPE), epichlorohydrin (ECO), polyvinylchloride (PVC), fluoroelastomers (FKM) and halobutyls (BIIR, CIIR). In many formulations, these additives have successfully replaced lead oxides without disrupting any processing or physical properties of the compounds. In addition, these antacids provide superior water swell compared to magnesium oxides in all the elastomers stated above. In most formulations, lead oxides will show slightly better water swell behavior compared to Sorbacid 911 (it may help to also use epoxidized soybean oil as plasticizer to help with acid acceptance). Sorbacid 911 can improve color of EPDM’s by scavenging the acid chlorides left over from the polymerization process. Sorbacid 911 also has a special attribute of an internal decomposition and water release from 260°C to 300°C acting as flame-retardant and smoke suppressant. This product has been added to other flame retardant systems as inorganic stabilizer and smoke suppressant, especially with halogenated systems. Sorbacid 911 is also utilized in electrical applications for their anti-tracking properties. Compounds that could not be colored brightly due to lead content can now be made using Sorbacid 911

Information provided by Akrochem Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.21 g/cc
Particle Size <= 1.0 µmAverage, d50
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 0.50 %
@Temperature 105 °C,
Time 7200 sec

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PAKZCH345 / 315263

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.